Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
Which spray nozzle for Pattern Coat Primer?
Which spray nozzle for Pattern Coat Primer?
Post Reply
Like
2
Which spray nozzle for Pattern Coat Primer?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
MarkMK
MarkMK
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 338,
Visits: 2K
Hi
My cup gun came with a FN6 nozzle suitable for gelcoats, but which is what is the ideal size for spraying the Pattern Coat and also the High Gloss finish?
Thanks
Mark
Reply
Like
2
Warren (Staff)
Warren (Staff)
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Yes you can spray the Pattern-Coat Primer by cup gun. Use the standard FN6 nozzle and thin down the Primer using 25% of pure acetone. That should thin it to a sprayable consistancy.
For the Pattern-Coat Hi Gloss, a
pplication by gelcoat spray gun will yield the best results and mean much less finishing work is required. When spraying, thin the Pattern-Coat™ Hi Gloss using
pure acetone
at a ratio of 25%.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search