Which spray nozzle for Pattern Coat Primer?
http://www.talkcomposites.com/Topic15045.aspx
By MarkMK
-
2/12/2015 12:02:35 PM
Hi
My cup gun came with a FN6 nozzle suitable for gelcoats, but which is what is the ideal size for spraying the Pattern Coat and also the High Gloss finish?
Thanks
Mark
By Warren (Staff)
-
2/12/2015 12:58:49 PM
Yes you can spray the Pattern-Coat Primer by cup gun. Use the standard FN6 nozzle and thin down the Primer using 25% of pure acetone. That should thin it to a sprayable consistancy.
For the Pattern-Coat Hi Gloss, a
pplication by gelcoat spray gun will yield the best results and mean much less finishing work is required. When spraying, thin the Pattern-Coat™ Hi Gloss using
pure acetone
at a ratio of 25%.