I'm about to take on my first infusion project, have been using prepreg and regular vacuum bagging to this point but this part is too big to fit in my oven. I'm confused as to how the resin flows from the spiral tubing into the reinforcement if the tubing is supposed to sit on top of the peel ply as all the tutorials say?
Reply
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
https://www.easycomposites.co.uk/peel-ply
Chris
Carbon fibre works LTD

PS using some of this between your mesh and peel ply will help when removing your infusion mesh.

Edited 10 Years Ago by carbonfibreworks
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search