Talk Composites - The Forum for Advanced Composites

How does resin get under the peel ply?

http://www.talkcomposites.com/Topic14907.aspx

By 360Challenge - 2/2/2015 6:02:02 PM

I'm about to take on my first infusion project, have been using prepreg and regular vacuum bagging to this point but this part is too big to fit in my oven. I'm confused as to how the resin flows from the spiral tubing into the reinforcement if the tubing is supposed to sit on top of the peel ply as all the tutorials say?
By VVS - 10/27/2015 9:38:05 AM

A little thing ive figured with peel ply is to think about the way you lay it when building your stack.

if you need to put strips in because of the complexity of the parts shape, run all your pieces of peel ply the same way so the red lines all go in the same direction.

it's around 50% easier to rip/remove when going with the red line and if you lay it with the lines running 90deg to each other it's a real bitch to get out.