Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
The unimould system can be applied by brush.
Reply
Like
3
kip
kip
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 32,
Visits: 99
Hanaldo (22/01/2015)
The unimould system can be applied by brush.
The gelcoat I got here is from a big composits factory here and they only had spray tipe vinyel ester gelcoat
Reply
Like
3
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Ahhh I see! My bad, I thought I had read that you were using unimould, now I see I totally made that up!
In any case, it still shouldn't give you release issues. The only issue I can see is that spray gelcoat is thinner than brush gelcoat and so it will be harder to brush it on to the appropriate thickness. However this would only cause issues with improper curing and alligatoring, I don't believe it would cause any issues with release.
What issues are you having now? Have you got a photo of your tray? Straight 0 degree edges on 4 sides would certainly cause release difficulties if the edges have enough surface area. If they are only small lips then it shouldn't be too bad, but if they are decent sized edges with a bit of surface area to create friction then releasing a part from them would be difficult.
Reply
Like
2
kip
kip
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 32,
Visits: 99
Well I thought its maybee because the products there are in the spray gelcoat to make it thinner ( aceton or styreni ) these could maybee make the polyester parts or the clear coat on some parts weak and thats why they wont release specially on the round edges .
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Prev
1
2
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search