By kip - 1/16/2015 12:37:43 AM
Hi,
I got some problems with the Easy-Lease Mould Cleaner .
I want to make new molds from vinylester gelcoat and resin for infusing and maybe later prepreg .
Before I always made my moulds from normal gelcoat and polyester resin so I used only wax what never gave any problems .
But now with the vinylester products I had problems demolding the moulds from the normal polyester parts with normal wax .
When I got the vinylester mould ready I infused some parts and it worked verry well no release problems with normal wax .
Now I wante dto make a new vinylester mould from a carbonfibre race parts and again the vinylester mould wouldn't release from the arnon fibre part .
So now I wanted to use the Easy-Lease Chemical Release Agent
I used a new polyester part I pulled from a old mould of me , polished it to mirror finish and then I cleaned it with the Easy lease mould cleaner and then the looked like the pics.
When I use the mould cleaner on a unpolished part it looks fine and stays the same look .
|
By kip - 1/23/2015 10:28:55 AM
Well I thought its maybee because the products there are in the spray gelcoat to make it thinner ( aceton or styreni ) these could maybee make the polyester parts or the clear coat on some parts weak and thats why they wont release specially on the round edges .
|
|