Finishing cured Kevlar / aramid edges


Author
Message
philiplardner
philiplardner
Supreme Being (546 reputation)Supreme Being (546 reputation)Supreme Being (546 reputation)Supreme Being (546 reputation)Supreme Being (546 reputation)Supreme Being (546 reputation)Supreme Being (546 reputation)Supreme Being (546 reputation)Supreme Being (546 reputation)
Group: Awaiting Activation
Posts: 25, Visits: 65
Hi,

What is the best way to cut / trim and finish the edges of Kevlar / aramid parts after demolding so that they do not end up with a 'furry' edge?

I am using a high speed Dremel-type tool with a diamond cutting disc (the carbide discs are too thin and delicate, and shatter too easily) to cut the cured Kevlar but it leaves a slightly fuzzy edge. Is there a way to finish these edges so that they have a cleaner finish (like sanded carbon edges)?

Thanks,

Phil.
                                                    
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Either sanding block as above or once youve achieved the correct edge profile, you can use a new razor blade to slice off any "fluff" on the edges.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search