By philiplardner - 1/12/2015 3:22:24 PM
Hi,
What is the best way to cut / trim and finish the edges of Kevlar / aramid parts after demolding so that they do not end up with a 'furry' edge?
I am using a high speed Dremel-type tool with a diamond cutting disc (the carbide discs are too thin and delicate, and shatter too easily) to cut the cured Kevlar but it leaves a slightly fuzzy edge. Is there a way to finish these edges so that they have a cleaner finish (like sanded carbon edges)?
Thanks,
Phil.
|
By philiplardner - 1/20/2015 10:33:26 AM
Thanks guys - I'll give those methods a try.
Much appreciated,
Phil. carbon-dragon.ihpa.ie
|
|