Hello,

the question is in the title, I'd like to know where to find a curing oven and how much does it costs.
I imagine that they are very expensive. Is there a more economical solution to make carbon parts with pre pregs?

Thanks in advance
Replies
JRT
JRT
Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)
Group: Forum Members
Posts: 13, Visits: 130
I have been reading all the posts regarding curing ovens in this forum.
I was wondering about how the vaccum and the fans work togheter, if the oven is on a vaccum status shouldn't it be without any air? If so what's the fan role?!
Thanks for all I've already learned here.
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
The part is under vacuum but the air inside the oven needs to be moved around to even out the heat, like a fan oven in the kitchen

JRT (05/01/2015)
I have been reading all the posts regarding curing ovens in this forum.
I was wondering about how the vaccum and the fans work togheter, if the oven is on a vaccum status shouldn't it be without any air? If so what's the fan role?!
Thanks for all I've already learned here.

JRT
JRT
Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)Supreme Being (97 reputation)
Group: Forum Members
Posts: 13, Visits: 130
ChrisR (05/01/2015)
The part is under vacuum but the air inside the oven needs to be moved around to even out the heat, like a fan oven in the kitchen


Ok, I see what you mean now and that makes sense. I´m planning on making one so I guess I should find some kind of fan that makes the air inside the oven to flow the heat around. The idea is to use it to do some post cure on the parts to give it more structural resistance.