posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 16,
Visits: 112
Hello,
the question is in the title, I'd like to know where to find a curing oven and how much does it costs.
I imagine that they are very expensive. Is there a more economical solution to make carbon parts with pre pregs?
Thanks in advance
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Where to find a curing oven
Adelbolide
-
12 Years Ago
> I'd like to know where to find a curing oven and how much does it costs. > I imagine that...
brainfart
-
12 Years Ago
I just purchased a couple of (damaged) lab ovens of ebay for a reasonable price. I will have to make...
scottracing
-
12 Years Ago
As above Ebay/bid spotter for bargins £200/£300 should get you going with a small bench top oven ....
f1rob
-
12 Years Ago
Thanks everybody for your help I'll look into it
Adelbolide
-
12 Years Ago
I have been reading all the posts regarding curing ovens in this forum. I was wondering about how...
JRT
-
11 Years Ago
The part is under vacuum but the air inside the oven needs to be moved around to even out the heat,...
ChrisR
-
11 Years Ago
[quote][b]ChrisR (05/01/2015)[/b][hr]The part is under vacuum but the air inside the oven needs to...
JRT
-
11 Years Ago
Easycomposites will have a suitable oven for sale shortly :) Chris Carbon fibre works LTD
carbonfibreworks
-
11 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search