Hi,k I have been skinning interior parts with 3k twill cloth, and have noticed in this cold weather it's taking a lot longer to cure. So I have put these parts beside my water heater. I am wondering what are the ideal conditions for curing and if say a plug in heater would help speed the cure.also, would a dremel be best to trim the edges off then sand? 
Next I am hoping to skin a spare set of wing mirrors, would the profinish fabric be flexible enough to wrap around it. As the normal fabric might be difficult to place
Thanks
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search