ANY IMAGE PLEASE WHERE YOU INSERT NEW PIECE OF CARBON WHERE ANGLE TO DIFFICULT?  how you do that so pattern is straight any video or photo?
Hanaldo
Hanaldo
Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
He is using set-weave carbon so it's much easier, but generally if you've got a shape that is too difficult to lay neatly without distorting the weave then you need to make relief cuts. Again, easier with set-weave fabric, but still possible to do with ordinary fabric if you are patient and gentle. 
TomDesign
TomDesign
Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
any luck with images how to do that? so that would help me a lot
Brian2fast
Brian2fast
Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)
Group: Forum Members
Posts: 79, Visits: 1.3K
I didn't take any photographs when I was laying the first layer of fabric I'm afraid. I'll try and explain how i did it.

http://www.talkcomposites.com/Uploads/Images/409f6838-8bb7-4ef8-9377-916b.JPG


I made paper templates for the shapes I would need for the first layer of Pro-finish fabric. The paper templates needed bigger edge relief cuts than the fabric did (as Hanaldo mentioned). Two edges of fabric would meet where my fingers are in the pic above. Instead of ragged join (I knew I would never get a neat join here) I used a strip of carbon spread tow (see link below). I put the spread tow in the mould first with spray glue, then the two bits of pro-finish fabric with the join hidden by the spread tow.

https://www.easycomposites.co.uk/80g-15mm-carbon-fibre-spread-tow-ribbon

The pro-finish fabric really makes things a lot easier for getting the weave nice and straight. It just doesn't drape around compound curves very good.

Hope that makes sense!
 

Craig
TomDesign
TomDesign
Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
so you say first piece to cut straight then next piece from other side if goes to do longer and simply to put on top of first yes? or simply cut to perfect 2 pieces and to try to get best join? sorry for my english
Hanaldo
Hanaldo
Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Nah overlap the second piece. So you only need to cut one piece perfectly (and to be honest, if you've got a couple of frayed fibres in there no one will ever notice unless you point it out), then the second piece can be longer and just sit over the top. If you are going for a v-weave join then you just want to make sure your weaves line up where it will be visible not where it overlaps. 
TomDesign
TomDesign
Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
Thank you a lot im going to try to do this. any advise if i want to do like this sheet- 1 layer 200gr cf then and Soric 3mm then 1 layer 200gr cf on the back. you think i get same result as here?

Hanaldo
Hanaldo
Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)Supreme Being (29K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Same result as in surface finish or thickness or what? 
TomDesign
TomDesign
Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
no im simply asking you think these cards he used what im thinking to lay or you think to thin? also he said those cards reason polished - but for what i know resin polished affraid on sun uv and all resin like that or i mistaken?
Brian2fast
Brian2fast
Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)Supreme Being (895 reputation)
Group: Forum Members
Posts: 79, Visits: 1.3K
A quick update. Today was the first time I have seen the new scuttle panel outside in sunlight and I spotted areas of white embedded within the resin. I know this is where I sprayed the Aerofix 3, so I'm sad to say I can see where this spray glue has been used. Its not that bad really and you need to know where to look for it but it is visible.

Warren, any more updates for the spray adhesive from the show?

Craig
Edited 12 Years Ago by Brian2fast
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search