I've got a kg of EL80 and I've been having a little play with some offcuts of cloth to see how it cures.  One thing I did notice is that its fairly viscous.  Is it OK to warm it a touch to thin it down a bit?

Would a review of my test pieces be of use?  If so I'd appreciate a few pointers of what people woould like to see.
Reply
FLD
FLD
Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
I thought I'd update this with a little 'how its holding up' post.

I've dragged the airdam over several sleeping policemen, up and down car park ramps etc and I can report that it has held up really well.  It just flexes (as you'd expect) but there is no real marks from the abrasions, not a sausage!  It has suffered from one fairly nasty stone chip which did leave some damage into the carbon.  IMO a rigid laminate wouldn't have been damaged to the same extent but its just a feeling I have rather than a quantifyable.   My overall verdict is that its awesome for low speed bending and abrasive resistance but it does suffer in high speed point impacts a little more.  Overall I'm pleased with it.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
FLD - 14 Years Ago
FLD - 14 Years Ago
Matt (Staff) - 14 Years Ago
FLD - 14 Years Ago
FLD - 14 Years Ago
matthieutje65 - 14 Years Ago
FLD - 14 Years Ago
FLD - 14 Years Ago
Matt (Staff) - 14 Years Ago
FLD - 14 Years Ago
FLD - 14 Years Ago
Matt (Staff) - 14 Years Ago
FLD - 12 Years Ago
Warren (Staff) - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search