Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Addition Cure Silicone Rubber
Addition Cure Silicone Rubber
Post Reply
Like
2
Addition Cure Silicone Rubber
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
JaWillis
JaWillis
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 8,
Visits: 24
Can this silicone be used to make a mold that can then be placed in an oven to cure pre-preg - oven temp will be 250F or 112C.
Thanks in advance to your reply
Reply
Like
2
20_rc51_00
20_rc51_00
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 95,
Visits: 548
these tend to be too flexible and rubber, they would deform under pressure as it's likely impossible to ensure there are no tension areas in a bagged part.....
I have heard of someone incorporating some sections made of these silicones in areas where complicated tabs and recess are needed for mounting motorcycle bodywork for example....
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search