By JaWillis - 10/27/2014 12:13:24 AM

Can this silicone be used to make a mold that can then be placed in an oven to cure pre-preg - oven temp will be 250F or 112C. 

Thanks in advance to your reply
By 20_rc51_00 - 10/27/2014 3:30:03 AM

these tend to be too flexible and rubber, they would deform under pressure as it's likely impossible to ensure there are no tension areas in a bagged part.....

I have heard of someone incorporating some sections made of these silicones in areas where complicated tabs and recess are needed for mounting motorcycle bodywork for example....