these tend to be too flexible and rubber, they would deform under pressure as it's likely impossible to ensure there are no tension areas in a bagged part.....

I have heard of someone incorporating some sections made of these silicones in areas where complicated tabs and recess are needed for mounting motorcycle bodywork for example....
JaWillis
JaWillis
Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)Forum Member (46 reputation)
Group: Forum Members
Posts: 8, Visits: 24
Can this silicone be used to make a mold that can then be placed in an oven to cure pre-preg - oven temp will be 250F or 112C. 

Thanks in advance to your reply
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search