jamesw
jamesw
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 61,
Visits: 558
I am planning to build a car nose cone with a split mould using infusion. I plan to infuse each half, then bond these halves together (soric core)
I'm looking for techniques and suggestions to accurately cut down and align the components for bonding... If anyone has tackled this before please let me know!
James
Reply
Like
2
Replies
jamesw
jamesw
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 61,
Visits: 558
The bonding thickness I'm not too worried about - It's trimming it accurately so it mates up properly - I can trim it in mould, but how to do it without damaging the tooling coat on the mould?!
Reply
Like
2
ChrisR
ChrisR
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 363,
Visits: 3K
Simples, very carefully!
You just need to mark up and cut so you have a few mm to spare then slowly and gently remove the material up to the mark but checking against the other part regularly.
You can take it away easily but it's messy to put back
or as the other saying goes, measure twice (or 5 times!) and cut once
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Techniques for bonding parts from a split mould....
jamesw
-
11 Years Ago
have any images of the nose?
kidpaint
-
11 Years Ago
If you use 2x200g cloth each side and a 3mm soric core you'll end up with a 4mm thick moulding. This...
FLD
-
11 Years Ago
The bonding thickness I'm not too worried about - It's trimming it accurately so it mates up...
jamesw
-
11 Years Ago
Simples, very carefully! You just need to mark up and cut so you have a few mm to spare then...
ChrisR
-
11 Years Ago
surely a joggle joint will be best ? than trying to join butt ends ?
Blackrat
-
11 Years Ago
If you use the excess flange material as a guide, you can get it very close to perfect without...
Hanaldo
-
11 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search