Group: Forum Members
Posts: 468,
Visits: 2.7K
|
If you use 2x200g cloth each side and a 3mm soric core you'll end up with a 4mm thick moulding. This should give enough area to bond directly. If you're worried you can then add some carbon tape down the inside to firm it up further.
|