Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
pre preg , resin not covering whole part "help please"
pre preg , resin not covering whole part "help please"
Post Reply
Like
2
pre preg , resin not covering whole part "help please"
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
ice2T
ice2T
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 7,
Visits: 159
Hello to all, I'm still at a very early learning stage with composites , but would grateful of some professional advice or guidance to help me along the way.
I am useing 1 layer of easy preg for what is seeming to be a very awkward part to get Wright . As the description says for use of the easy preg is to oven cure for ten hours at 100c ' I have followed this instructions but 5 parts later I am still getting generally the same outcome of the parts. I have been looking on the forum for information of people with the same problems . What keeps popping up is a lot of people are talking about ramping up and down in the curing process.
So this is what I did I cured the part for 6 hours instead of ten , I started at 30c 1hr/50c1hr/75c1hr/60c1hr/ and you wouldn't believe it from the pictures but it actually came out better. As I am at loss now of what to do next please could anyone "Or everyone...lol help .....
Reply
Like
2
Replies
Matthieu Libeert
Matthieu Libeert
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
as above, are you leaving your vacuum on?
You need to keep the pump running for better results.
As well do you have a perfect sealed bag?
Without a well sealed bag you dont even have to start the curing because you'll keep getting bad results.
How is the surface of your mould?
as for the curing cycle try following: 3hours 65°C, 2hours 85°C, 2hours 105 °C, 1hour 115°C.
as above the change between temperatures should be slow and steady, if you are working with a kitchen oven this will be
more difficult
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
ice2T
ice2T
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 7,
Visits: 159
Hi this is the sursurface of the the mold which is constructed useing the uni mold system and seems to have a a good finish , I also had thoughts that because having full vacume all way through the curing cycle that the vacume could be pulling the resin off the part before being able to set....?
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
pre preg , resin not covering whole part "help please"
ice2T
-
11 Years Ago
I'm possibly not the best person to comment as I haven't personally used pre-preg before, but from...
Hanaldo
-
11 Years Ago
Hi my friend thankyou for your reply which is very welcome , What you're saying about the...
ice2T
-
11 Years Ago
Hi my friend thanks for your reply it is very welcome , I'm going to try and control the ramping via...
ice2T
-
11 Years Ago
Again, I am not an expert but I don't think your ramp up/down time should be taken away from the...
Brian_s
-
11 Years Ago
as above, are you leaving your vacuum on? You need to keep the pump running for better results. As...
matthieutje65
-
11 Years Ago
Hi this is the sursurface of the the mold which is constructed useing the uni mold system and seems...
ice2T
-
11 Years Ago
Thanks my friend for advice, yes I'm going to try putting it back up to the ten hours but slow the...
ice2T
-
11 Years Ago
When using prepreg you typically use a non perforated release film so it doesn't bleed the resin out...
ChrisR
-
11 Years Ago
You don't mention which pre-preg you are using our Easy-Preg Surface layer or normal Vari-preg?...
Warren (Staff)
-
11 Years Ago
Hi Warren I'm the chap that went outside to look at your bonnet on your car in the car park if you...
ice2T
-
11 Years Ago
So a single layer of Easy Preg surface layer with no backing? If so you may find that is causing...
Warren (Staff)
-
11 Years Ago
Ok my friend , ill give it a shot makes sense.....cheers
ice2T
-
11 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search