David Linton
David Linton
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2,
Visits: 48
andygtt you are a GOD!
The work carried out is amazing and really inspires me to get moving with some of my own projects. Keep up the good work dude.
Reply
Like
2
andygtt
andygtt
posted 10 Years Ago
ANSWER
Post Details
Group: Forum Members
Posts: 157,
Visits: 1.2K
macgtech (16/07/2014)
Thoroughly enjoyed going through this - great job.
What weight saving have you seen by going down the full CF route?
45kgs in the carbon bodywork... but Ive saved another 20 kgs in general 'stuff' that was on the car under the tub (wiring, brackets, nuts and bolts) that didn't do anything and were just dead weight.
Im planning on making my own seats soon and am replacing the alloy flooring under the car with carbon so there is still a little more planned... my single turbo engine package and clutch package also saved me quite a bit of weight over a standard car. so I'm actually 100kgs lighter than other well modified nobles (going up in power adds around 50kgs to the car due to intercoolers, extra rads etc etc)
I run a motec M800 ecu and mapped some of the advanced settings the other day to unleash the boy racer in me
https://www.youtube.com/watch?v=kC0Phc1SUvw
Reply
Like
1
FLD
FLD
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 2.7K
Hanaldo (16/07/2014)
I appreciate the offer, but I'm in Australia!
Ah, that'd be a problem. :lol:I also cut out sections of the inner to reduce weight leaving a figure eight shapped inner. I'd be inetersted to see how you get on.
Reply
Like
2
macgtech
macgtech
posted 10 Years Ago
ANSWER
Post Details
Group: Forum Members
Posts: 20,
Visits: 102
Thoroughly enjoyed going through this - great job.
What weight saving have you seen by going down the full CF route?
MacG Racing Ltd.
, UK based Motorsport Racing Team - follow us on
Twitter
and on
Facebook
Reply
Like
1
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
I appreciate the offer, but I'm in Australia!
I also need to modify this one a little bit. The car has a custom made lightweight windscreen with internal heating which is a different size to the standard windscreen, so there is a 20mm gap between the stock fibreglass roof and the windscreen. So I'll be modifying the roof to bring it back down and sit under the seal again. I also need to find 10-15mm of extra headroom as the driver currently hits his head, so I'll likely be chopping a large section of the inner skin out.
Reply
Like
2
FLD
FLD
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 2.7K
If it helps I made a VX220 roof. I have the mould for the inner part which may be similar.
Reply
Like
2
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Thanks Andy.
I've had a look at the car I'm doing now, starting the job next week most likely. Luckily the Exige roof is not as big a job as this, it is really more of a bonnet. Will be a 2 piece mould with an inner and outer skin. Surface area is roughly 1sqm, so not very big either.
Reply
Like
2
andygtt
andygtt
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 157,
Visits: 1.2K
Sorry for not seeing this earlier, got married and thus was a little busy
Id estimate its cost me in materials around £10k to do my entire car, that includes the mould materials, consumables and 'learning' curve errors... and included in that a small stockpile of materials left over to make more parts.
to make the front clam for my car from the now existing moulds it cost me around £700, but it takes 3 days min before trimming, lacquering etc etc.
The mould process and material is actually the most expensive part
Reply
Like
2
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Thanks for the reply Warren. That is exactly what I will do when I get the chance to see the car and measure things, I just like to have a rough idea in my head before I go do quotes but I'm operating with no real idea on surface area at the moment. No big deal, I just like to be organised.
I did manage to find pretty much exactly the same job has been done by Nitron in the UK. Looking at their pictures, it looks like it will actually be closer to a bonnet than what Andy has done here anyway.
Reply
Like
1
Warren (Staff)
Warren (Staff)
posted 10 Years Ago
ANSWER
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8K
There never is any simple way to estimate costs.
You have to do the maths. In essence think of your mould in terms of surface area of the part and flanges.
You then need the number of layers of carbon, core etc,
calculate the resin usage here:
http://www.talkcomposites.com/11/Resin-infusion-resin-usage-calculation
Then add your consumables to get a rough material cost.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
1
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
1
2
3
4
5
8
Next
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search