Hello!

I have a question about  sandwich core technique.
That is...

For example,
If I use  two set of  5mm nomex honeycomb core(10mm thick in total) to  make a sandwich panel,
is it  as strong as  a single 10 mm nomex honecomb core panel?
the  double 5mm sandwich has reasonable strength?
or the double 5mm sandwich is easy to break?


actually,
I want to build a curved sandwich panel.
I tried a 10mm thick  nomex honeycomb core at first,
but the 10mm thick core was too strong to bend.

 I wonder that if I use  a 5mm core,then laminate,bend  and add one more 5mm honeycomb core.
I mean,,  the sandwich is   CFRP>honeycomb core(5mm)>CFRP>honeycomb core(5mm)>CFRP.
If this idea is O.K. I will be able to build thick and strong curved sandwich panels.


Any advice,
I would be happy.

Thanks,







 
Reply
hietaka
hietaka
Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)Supreme Being (118 reputation)
Group: Forum Members
Posts: 14, Visits: 169
>> Warren san,

Your advice is very helpful and informative!  many thanks!


well...It seems that
I should be careful about a direction of loading.
loading on a bended CFRP>sandwich panel may cause  inside separation...
hum...
using bended sandwich panel is not that good idea, I feel.
If possible, I should look for a different choice.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
hietaka - 12 Years Ago
Warren (Staff) - 12 Years Ago
hietaka - 12 Years Ago
brainfart - 12 Years Ago
brainfart - 12 Years Ago
hietaka - 12 Years Ago
Warren (Staff) - 12 Years Ago
f1rob - 12 Years Ago
hietaka - 12 Years Ago
f1rob - 12 Years Ago
brainfart - 12 Years Ago
ChrisR - 12 Years Ago
Warren (Staff) - 12 Years Ago
hietaka - 12 Years Ago
hietaka - 12 Years Ago
Warren (Staff) - 12 Years Ago
hietaka - 12 Years Ago
f1rob - 12 Years Ago
hietaka - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search