By hietaka - 7/7/2014 3:48:19 PM
Hello!
I have a question about sandwich core technique. That is...
For example, If I use two set of 5mm nomex honeycomb core(10mm thick in total) to make a sandwich panel, is it as strong as a single 10 mm nomex honecomb core panel? the double 5mm sandwich has reasonable strength? or the double 5mm sandwich is easy to break?
actually, I want to build a curved sandwich panel. I tried a 10mm thick nomex honeycomb core at first, but the 10mm thick core was too strong to bend.
I wonder that if I use a 5mm core,then laminate,bend and add one more 5mm honeycomb core. I mean,, the sandwich is CFRP>honeycomb core(5mm)>CFRP>honeycomb core(5mm)>CFRP. If this idea is O.K. I will be able to build thick and strong curved sandwich panels.
Any advice, I would be happy.
Thanks,
|
By hietaka - 7/22/2014 3:43:43 PM
>f1rob san
Thanks! I searched the 1-5 CFRP items. The CFRP furniture is so stylish!
I think I should continue to design the CFRP wheelchair. I believe that I can improve wheelchair.
I will post again if my design is finished.
|
|