Hi Guys,
Wondered if anyone had post cured any of their resin infused parts?
I see on the EC website/shop under technical questions, thereis a little on the subject saying that you can post cure IN2 resin to raise the heat distortion temp.
My part needs to be good for up to 80 degrees C
Many thanks
Brett
Thanks for all the suggestions. Its nice to know that i can work with the IN2 resin and not have to buy in special high temp stuff!