Hi Guys,

Wondered if anyone had post cured any of their resin infused parts?

I see on the EC website/shop under technical questions, thereis a little on the subject saying that you can post cure IN2 resin to raise the heat distortion temp.

My part needs to be good for up to 80 degrees C