Post curing IN2 infusion resin.

http://www.talkcomposites.com/Topic11974.aspx

By brettalloy - 6/23/2014 10:55:24 AM

Hi Guys,

Wondered if anyone had post cured any of their resin infused parts?

I see on the EC website/shop under technical questions, thereis a little on the subject saying that you can post cure IN2 resin to raise the heat distortion temp.

My part needs to be good for up to 80 degrees C

Many thanks

Brett

By brettalloy - 6/25/2014 11:33:30 AM

Thanks for all the suggestions. Its nice to know that i can work with the IN2 resin and not have to buy in special high temp stuff!