Need help with Base Coat on CF Skinning


Author
Message
SuperFastYo
SuperFastYo
Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)
Group: Forum Members
Posts: 4, Visits: 9
New to the forum and would greatly appreciate any help! I am having a bit of trouble with skinning my interior trim (aluminum) with CF. Whenever I lay the base coat down it begins to pool and pull away from the trim. I have sand with 120 which didnt work so I went to 100 and that still hasnt worked. Finally I went to 80 and even though the surface is throughly sanded, it will not stay in place. Any advice?


Replies
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
TargaMustang
TargaMustang
Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)
Group: Forum Members
Posts: 8, Visits: 51
TomDesign (18/06/2014)
yes sure man . i do tons of wraps so i know what i say Smile




So what is it??  A wax and grease remover?  I can't find an English translation of what it is.