Talk Composites - The Forum for Advanced Composites
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - Product Specific Pages
»
Carbon Fibre Cloth Fabric
Need help with Base Coat on CF Skinning
http://www.talkcomposites.com/Topic11891.aspx
By SuperFastYo
-
6/18/2014 5:40:19 AM
New to the forum and would greatly appreciate any help! I am having a bit of trouble with skinning my interior trim (aluminum) with CF. Whenever I lay the base coat down it begins to pool and pull away from the trim. I have sand with 120 which didnt work so I went to 100 and that still hasnt worked. Finally I went to 80 and even though the surface is throughly sanded, it will not stay in place. Any advice?
By SuperFastYo
-
6/18/2014 3:52:22 PM
brainfart (18/06/2014)
Sure, give it a try.
Lol that's not very reassuring. Jk, I'll try later today and report back.