Group: Forum Members
Posts: 346,
Visits: 4.4K
|
You can do it without using either, run the resin in tube between the gum tape and vac bag with a ring of tape around, then use some spiral stuffed in the end to stop it collapsing. Have a piece of spiral taped all across the part and place the bit of spiral sticking out the tube on top of the spiral line
|