I was using acetone initially but it seemed to take the surface off the gel coat...so I used a rag and soap.
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Scrape most of it off with a popstick or similar, then give it a quick wipe with MEK (NOT MEKP) or acetone. 
BlackNDecker
BlackNDecker
Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)
Group: Forum Members
Posts: 92, Visits: 251
Great news!!!!!




Now does anybody have any pointers for getting the wax out?
Alibro
Alibro
Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)
Group: Forum Members
Posts: 44, Visits: 384
BlackNDecker (02/05/2014)
ajb100 (02/05/2014)
What % MEKP did you use? 

I used 1.5% MEKP in 1 gallon of gel coat...so going by the spec sheet (1% = 1 oz MEKP per 1 gallon gel coat), I used 1.5 oz of MEKP since it was a pretty chilly day. The spec sheet says you can add up to 2.0% or more depending on the temp.


Hi B&D
I am a complete amateur like yourself but I'm not sure about your maths here. I just checked and there are 160oz in an imperial gallon and 133oz in a US gallon.
Which was it you were working with US or Imperial gallons? Either way you were not as catalysed as you thought.
If I were you I would stick with grams and kg as the maths is much easier. Smile


 
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Due to the shape and size of the door, it might be worth adding two wide bits of wood into the laminate so that when you come to make it, you can rest it down and stop it from rocking. It will also make them much more rigid.

Just for future reference, unless you're making it a van, you don't need to mould the window opening, you can leave it open to save quite a bit of time and money/materials when you add up all 4 doors

Are you going to add any anti intrusion to the doors?
BlackNDecker
BlackNDecker
Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)
Group: Forum Members
Posts: 92, Visits: 251
Laid down the woven roving...got it as thick as 3 layers around the door sills. I am now out of supplies and out of energy. Hopefully everything turns out well.

Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Looking good mate. I use woven rovings on my moulds too. Very solid stuff. Bit hard to work with on small moulds, but you'll be right on a mould that size. Fingers crossed you don't get release issues now! Haha.
BlackNDecker
BlackNDecker
Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)
Group: Forum Members
Posts: 92, Visits: 251
Thanks fellas! Your input is GREATLY appreciated.

So I'm progressing right along...coupling coat and 3/4 oz mat:


And used a roller to press it in the corners.


Next up is a couple layers of 1.5 oz mat and polyester resin. For the final layer of laminate I'm planning to use this:
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
I wouldn't worry about orange peel anyway, you can flat that out with 1200 after. 
The Fibreglass King
The Fibreglass King
Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)
Group: Forum Members
Posts: 69, Visits: 652
Hi blackNdecker,
                                 It does make quite a bit of difference to the gel coat if it's not applied at the optimum temperature. It will most definitely need more gel to cover an area thus be harder to even out because  it's thick and you have to much gel on the surface.  Your gel was probably be colder than the ambient  temperature aswell! As for seeing Orange  peel under a second coat it would  almost impossible to tell if you have a really thick  layer of gel!  But saying all of that your gel coat looks a lot  tidier 😁 
                                                                                                  Kind Regards
                                                                                           The Fibreglass King
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search