You want to build the mold with West epoxy and apply it to the coupling coat?
You better do a small experimental mold first, I am not sure this will work. The uni-mould system uses a vinylester tooling gelcoat and both the coupling coat and tooling resin are polyester based. I am not sure the West will properly bond to them.

[Edit: typo]
Edited 11 Years Ago by brainfart
BlackNDecker
BlackNDecker
Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)
Group: Forum Members
Posts: 92, Visits: 251
D-day goes down on Friday...


This epoxy resin should be compatible with the Easycomposites coupling coat? I also have high quality polyester resin in case it's not....gotta read up more on the characteristics of the coupling coat.

BlackNDecker
BlackNDecker
Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)
Group: Forum Members
Posts: 92, Visits: 251
Thanks Hanaldo!

I went back and cleaned up the fillet wax and straightened up all the lines so that my cut lines will be easier to see. I'll start on the PVA tomorrow.
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Do 5-6 coats of release wax, 2-3 mist coats of PVA and then 1-2 heavier coats of PVA. 
BlackNDecker
BlackNDecker
Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)
Group: Forum Members
Posts: 92, Visits: 251
The fillet wax arrived and I massaged it into all crevices:


All done:


I got one good coat of Meguiars wax laid down before the fillet wax. Now I'm thinking I will spray 5-6 coats of PVA then give another try with the gel coat.
Edited 11 Years Ago by BlackNDecker
The Fibreglass King
The Fibreglass King
Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)
Group: Forum Members
Posts: 69, Visits: 652
Hi blackNdecker,
                                When you apply the gel coat start from the top and work down, dip your brush in the gel and dab a couple of splodges on,then brush across horizontaly then repeat this as you go down the door once it is all covered then strike down vertically and evenly this will take any excess gel to the bottom then return the excess gel to the pot! Leave for a couple of hous at least then repeat!! Hope this helps??       
                                                                             Kind Regards
                                                                        The Fibreglass King
BlackNDecker
BlackNDecker
Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)
Group: Forum Members
Posts: 92, Visits: 251
Lol...thanks.

My concern now is trying to apply gelcoat to a vertical surface:-[
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
nice poker game Smile

btw trust me doors not go bad they taken or mounted as they oem. so far so good with flange. remember good wax always correct ratio of hardener and try not to put hudge amount of gelcoat in places to look like dalmantin Smile
Devin Wang
Devin Wang
Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)Forum Member (28 reputation)
Group: Awaiting Activation
Posts: 4, Visits: 28
AD

Hey All:

Do you want to import FIBERGLASS & RESIN from China? we are your NO.1 choice.

This is Devin Wang from China CNBM(China National Building Material Corporation),a national owned company,14 years experience in the FRP material manufacturing.Our group owns more than 40 factories manufactured FRP material(fiberglass & Resin) through out China.

1)FIBERGLASS

  • E-glass fiber direct roving                      - Fob Shanghai USD 760/Metric Ton    
  • E-glass fiber gun roving                         - Fob Shanghai USD 1060/Metric Ton
  • E-glass fiber Chopped Strand Mat(powder &emulsion)         - Fob Shanghai USD 1330/Metric Ton
  • E-glass fiber Woven Roving                   - Fob Shanghai USD 960/Metric Ton

2)RESIN

  • Unsaturated Ployester Resin(including Gelcoat resin,Vinyl Ester resin)
  • Epoxy Resin

As to Resin price,we need your specification to confirm the prices.

Welcome to inquiry!

Best Regards,

Devin Wang/Sales Manager
CNBM/Composite Material Dept.


Address:Floor 17th, No.4 Building, Zhuyu International Commercial Center, No.9, Shouti South Road,Haidian District, Beijing 100048, China
Tel:+86-519-83982873
Mobile:+86-13584510068
Fax:+86-519-83982891
E-mail:devinwang@okorder.com
Website:www.icnbm.com,www.okorder.com


BlackNDecker
BlackNDecker
Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)
Group: Forum Members
Posts: 92, Visits: 251
I decided to mount the door on the car to mold it...it would've been heart breaking to mold a warped door:o)



I was hoping to get some feed back on my flanges. I used styrofoam poster board and playing cards.


Then I carefully taped the cards with foil tape:


And all finished up...I'm just waiting on the wax fillet I ordered from easy composites: