Trying to mold my doors...:((((


Author
Message
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
nice poker game Smile

btw trust me doors not go bad they taken or mounted as they oem. so far so good with flange. remember good wax always correct ratio of hardener and try not to put hudge amount of gelcoat in places to look like dalmantin Smile
BlackNDecker
BlackNDecker
Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)
Group: Forum Members
Posts: 92, Visits: 251
Lol...thanks.

My concern now is trying to apply gelcoat to a vertical surface:-[
The Fibreglass King
The Fibreglass King
Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)
Group: Forum Members
Posts: 69, Visits: 652
Hi blackNdecker,
                                When you apply the gel coat start from the top and work down, dip your brush in the gel and dab a couple of splodges on,then brush across horizontaly then repeat this as you go down the door once it is all covered then strike down vertically and evenly this will take any excess gel to the bottom then return the excess gel to the pot! Leave for a couple of hous at least then repeat!! Hope this helps??       
                                                                             Kind Regards
                                                                        The Fibreglass King
BlackNDecker
BlackNDecker
Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)
Group: Forum Members
Posts: 92, Visits: 251
The fillet wax arrived and I massaged it into all crevices:


All done:


I got one good coat of Meguiars wax laid down before the fillet wax. Now I'm thinking I will spray 5-6 coats of PVA then give another try with the gel coat.
Edited 11 Years Ago by BlackNDecker
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Do 5-6 coats of release wax, 2-3 mist coats of PVA and then 1-2 heavier coats of PVA. 
BlackNDecker
BlackNDecker
Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)
Group: Forum Members
Posts: 92, Visits: 251
Thanks Hanaldo!

I went back and cleaned up the fillet wax and straightened up all the lines so that my cut lines will be easier to see. I'll start on the PVA tomorrow.
BlackNDecker
BlackNDecker
Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)Supreme Being (630 reputation)
Group: Forum Members
Posts: 92, Visits: 251
D-day goes down on Friday...


This epoxy resin should be compatible with the Easycomposites coupling coat? I also have high quality polyester resin in case it's not....gotta read up more on the characteristics of the coupling coat.

brainfart
brainfart
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 198, Visits: 1.4K
You want to build the mold with West epoxy and apply it to the coupling coat?
You better do a small experimental mold first, I am not sure this will work. The uni-mould system uses a vinylester tooling gelcoat and both the coupling coat and tooling resin are polyester based. I am not sure the West will properly bond to them.

[Edit: typo]
Edited 11 Years Ago by brainfart
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
I have used epoxy as the tooling resin on a polyester gelcoat with one layer of 225 csm and polyester resin as a 'coupling' layer, and that worked fine. Obviously different combinations though, so I would also recommend doing a test first. 

However, if you've got the polyester resin, why not use that? 
The Fibreglass King
The Fibreglass King
Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)
Group: Forum Members
Posts: 69, Visits: 652
Hi, BlackNdecker,
                                  I would also go for the polyester resin! What lay up are going to use for the mould??
                                                                                             Kind Regards
                                                                                       The Fibreglass King