Hi,

In the last video EC uploaded, that you can see here, they use a polyester gelcoat (compatible with epoxy) that will be available as soon as they can make it.

Dunno if its what you want, but thats the way i understand "in mould coating". Hope it helps.

 



 


    A $1000 electronic device will always protect a 10 cents fuse
marc37i
marc37i
Supreme Being (164 reputation)Supreme Being (164 reputation)Supreme Being (164 reputation)Supreme Being (164 reputation)Supreme Being (164 reputation)Supreme Being (164 reputation)Supreme Being (164 reputation)Supreme Being (164 reputation)Supreme Being (164 reputation)
Group: Forum Members
Posts: 16, Visits: 566
Hi,

Could anyone recommend a good, easily available In Mould Clear coating? and one that is compatible with the EL2 and IN2 resins from EC.

I have found a 2k polyurethane product from HP-Textiles ( http://www.hp-textiles.com/shop/product_info.php?info=p770_750g-in-mould-coating---hp-imc-.html Wink, but they are based in Germany and I would prefer a UK based supplier(perhaps EC could add this product? :-) )

Many Thanks
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search