Bought laminating resin instead of infusion resin ,
Bought laminating resin instead of infusion resin ,
Post Reply
Like
3
Bought laminating resin instead of infusion resin ,
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
whereismillar
whereismillar
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 10,
Visits: 31
Hi
bought laminating resin instead of infusion resin , will this still work as an infusion resin?
or best to replace?, it is for a carbon bicycle frame repair BTW,
andy
Reply
Like
3
Reply
Matthieu Libeert
Matthieu Libeert
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
Hi Andy,
For a frame repair I would go for the laminating resin... So you dont need to change it!
Unless you are repairing the frame with infusion but I would highly doubt that
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Bought laminating resin instead of infusion resin ,
whereismillar
-
11 Years Ago
Hi Andy, For a frame repair I would go for the laminating resin... So you dont need to change it!...
matthieutje65
-
11 Years Ago
Hi matthieu I bought laminating resin but got the high temp stuff thinking a bike sitting in the...
whereismillar
-
11 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search