Bought laminating resin instead of infusion resin ,
http://www.talkcomposites.com/Topic10950.aspx
By whereismillar
-
4/25/2014 8:51:07 PM
Hi
bought laminating resin instead of infusion resin , will this still work as an infusion resin?
or best to replace?, it is for a carbon bicycle frame repair BTW,
andy
By whereismillar
-
4/29/2014 10:30:40 PM
Hi matthieu
I bought laminating resin but got the high temp stuff thinking a bike sitting in the sun may need it, doh!
so i have ordered standard (EL2)
thanks for the reply
all the best
andy