Bought laminating resin instead of infusion resin ,


Author
Message
whereismillar
whereismillar
Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)
Group: Forum Members
Posts: 10, Visits: 31
Hi matthieu

I bought laminating resin but got the high temp stuff thinking a bike sitting in the sun may need it, doh!

so i have ordered standard (EL2)

thanks for the reply

all the best

andy
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Hi Andy,

For a frame repair I would go for the laminating resin... So you dont need to change it!
Unless you are repairing the frame with infusion but I would highly doubt that

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




whereismillar
whereismillar
Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)
Group: Forum Members
Posts: 10, Visits: 31
Hi 
bought laminating resin instead of infusion resin , will this still work as an infusion resin?
or best to replace?, it is for a carbon bicycle frame repair BTW, 

andy