I have a loan of a wing to mould.  My last wing I moulded in two parts (top and bottom obviously!).  I flanged it across the front which gives a 90 degree angle.  Should I go beyond the split line and radius the mould so I can infuse easier?  The other option would just be what I've already done so can I infuse OK with the 90 degree angle?
Reply
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
Sorry, should've been clear; same with mine, I was just unsure how to do the ends of the mould (plan is to build out a bit with wax).