By FLD - 3/11/2014 8:28:37 PM
I have a loan of a wing to mould. My last wing I moulded in two parts (top and bottom obviously!). I flanged it across the front which gives a 90 degree angle. Should I go beyond the split line and radius the mould so I can infuse easier? The other option would just be what I've already done so can I infuse OK with the 90 degree angle?
|
By FLD - 3/13/2014 5:39:34 PM
Sorry, should've been clear; same with mine, I was just unsure how to do the ends of the mould (plan is to build out a bit with wax).
|
|