Bodykit making question


Author
Message
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
you think after 1 layer 300 2 layer 600 you think parts be stable and not weight a lot? as main thing for me not be very flexible and not to weight like a wall.
The Fibreglass King
The Fibreglass King
Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)
Group: Forum Members
Posts: 69, Visits: 652
Hi Tom,
               Mat is correct I gave you the weights off the c.s.m in grams and ounces / metric and imperial, these are set weights for grades of chopped strand mat that I recommend hope this helps?

                                                                                          Kind Regards
                                                                         .          The Fibreglass King.
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
As far as I know he gave you all the info in grams and ounce Smile

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
King please explain in euro not o Sad

i thought to lay one in 140gr or like 35gr then sand then 3 layers 380gr and extra 2-3 where flexible lines go or to put hard form ?
The Fibreglass King
The Fibreglass King
Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)Supreme Being (501 reputation)
Group: Forum Members
Posts: 69, Visits: 652
Hi Tom, 
              I would recommend using a 300gram/1 ounce chopped strand mat skin coat letting it completely cure, then give it a light sanding for a mechanical key, Then lay it up with  two layers of 600g / 2oz  then add 2oz strips in straregic places for extra strength or you could choose a lighter lay up 1oz skin / 3mm core mat / 1 1/2 oz over lay this would give the bodykit a good ridgity!!
                                                                                                   Kind regards
                                             .                                              The Fibreglass king
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
here are the parts before molding so you can imagine. http://www.talkcomposites.com/Uploads/Images/3dee4196-a56f-4c78-973b-46a3.JPG

im thinking maybe 3 layers frp and where lines of fenders go and other not stable places maybe tocut not width lines of same frp and to lay couple layers maybe to add line of foam hard . what you think guys?
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
My kit-car body is about 3-5mm thk CSM and flexes slightly, lots of curves in there though, they used to make it 7mm thk and solid as a rock but it was soo heavy
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
It all depends on the size and shape of the parts, the more curves and swage lines, the less you'll need
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
Hello

guys i be making full widebodykit for me. can anyone suggest how many layers and what to put best so to be good in weight also to be strong and not to flexible.

Bodykit be made from fiberglass.

1.front bumper
2. front fenders set
3. hood
4. side skirts set
5. doors skins set
6. rear fenders set
7. rear bumper
8. canards set
9. wing
10. wing extra small one 