something I've been working on the past week. its a brake master cylinder cover.
I need to produce a lot of these, i resin infused this one last night but took me around an hour and half. (I'm still new to all this)
What would be the easiest/quickest way? and keeping the cost down

Thanks








Reply
Darren
Darren
Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)Supreme Being (406 reputation)
Group: Forum Members
Posts: 54, Visits: 916
Ok i know which way im going with this now Wink

Another question, whats the best spray adhesive that is ok to use with epoxy? and won't dissolve my release agent?
The mould is quite deep and has tight curves so want something to hold fabric in place
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Darren - 11 Years Ago
ajb100 - 11 Years Ago
FLD - 11 Years Ago
matthieutje65 - 11 Years Ago
Darren - 11 Years Ago
ajb100 - 11 Years Ago
Darren - 11 Years Ago
ajb100 - 11 Years Ago
Darren - 11 Years Ago
ajb100 - 11 Years Ago
Darren - 11 Years Ago
ajb100 - 11 Years Ago
                     I use Aerofix2 as well and works perfect!