something I've been working on the past week. its a brake master cylinder cover.
I need to produce a lot of these, i resin infused this one last night but took me around an hour and half. (I'm still new to all this)
What would be the easiest/quickest way? and keeping the cost down

Thanks








Replies
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Darren (07/03/2014)
ajb100 (06/03/2014)
I use aerofix 2, a lot suggest 3m 77 but I find it hard to get and expensive 


Do you have any probs with part release? and what release agent are you using?


No release problems at all. Generally I'll use easy lease with a layer or two of wax on top
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
I use Aerofix2 as well and works perfect!

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Darren - 11 Years Ago
ajb100 - 11 Years Ago
FLD - 11 Years Ago
matthieutje65 - 11 Years Ago
Darren - 11 Years Ago
ajb100 - 11 Years Ago
Darren - 11 Years Ago
ajb100 - 11 Years Ago
Darren - 11 Years Ago
ajb100 - 11 Years Ago
Darren - 11 Years Ago
ajb100 - 11 Years Ago
                     I use Aerofix2 as well and works perfect!