I'm havin trouble with my first infusion where iv got a tiny air leak sumwhere and I can't find it.
Iv even ripped the bag off it and started again making sure to be carefull sticking it dwn to the gum but still the same 
my question is 
Is there a certain way to not get leaks or should I just get a ultra sonic detector
Thanks
Reply
justas
justas
Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)
Group: Forum Members
Posts: 8, Visits: 65
The problem was in wrong vacuum film. After infusion resin ate out some micro holes in minutes. I both one from composites seller but with no any data sheet. After contacting they explained that is vacuum film for general usage Smile. Now I changed it and test is good. 2m fiberglass tube with polyester resin infusion one inlet at one end bottom of tube and one outlet on other end top with spiral across the tube took 30min.

http://www.talkcomposites.com/Uploads/Images/3368d559-af84-4416-ae17-95f6.JPG http://www.talkcomposites.com/Uploads/Images/ef83e33e-d2f1-4f22-8fab-89ed.JPG
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Jdmleesy - 11 Years Ago
morepower - 11 Years Ago
fgayford - 11 Years Ago
Pro-Comp - 11 Years Ago
carbonfibreworks - 11 Years Ago
Jdmleesy - 11 Years Ago
Dravis - 11 Years Ago
carbonfibreworks - 11 Years Ago
Jdmleesy - 11 Years Ago
fgayford - 11 Years Ago
andygtt - 11 Years Ago
ajb100 - 11 Years Ago
fgayford - 11 Years Ago
Jdmleesy - 11 Years Ago
fgayford - 11 Years Ago
justas - 11 Years Ago
fgayford - 11 Years Ago
Jdmleesy - 11 Years Ago
carbonfibreworks - 11 Years Ago
Jdmleesy - 11 Years Ago
     Bagging
Jdmleesy - 11 Years Ago
Warren (Staff) - 11 Years Ago
Jdmleesy - 11 Years Ago
justas - 11 Years Ago
fgayford - 11 Years Ago
Fasta - 11 Years Ago
justas - 11 Years Ago
ChrisR - 11 Years Ago
justas - 11 Years Ago
                         Normal 0 false false false EN-GB X-NONE X-NONE...
ChrisR - 11 Years Ago
justas - 11 Years Ago
justas - 11 Years Ago
justas - 11 Years Ago
macgtech - 11 Years Ago
justas - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search