Group: Forum Members
Posts: 346,
Visits: 4.4K
|
Have to agree with Fred, the white plastic infusion mesh is a paint to get to form to a mould and the edges punctured the bag. I went for a short time wrapping the edges in masking tape until I started using a different mesh and not had any problems since
|