Hi, I am new to composite stuff.
I am trying to make a small carbon fiber part. But when I lay down my first layer of resin, it doesn't get tacky. I waited for more than 20 mins. I am using Silmar 249A polyester surfboard resin. Does this resin ever get tacky?
Thanks
ajb100
ajb100
Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)Supreme Being (4.3K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
What percentage MEKP did you use and what was the ambient temp?
Warren (Staff)
Warren (Staff)
Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Not being one of our resins, I cant be sure what has gone on.

However, in general terms of normal polyester resins, There should definitely be a tack stage.  Did it go off at all??

Check your catalyst ratio very carefully and also consider the temperature of the environment you are working in. The colder it is the longer it takes to go off and in extreme cases temperature can stop it curing at all.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
yudif
yudif
Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)
Group: Awaiting Activation
Posts: 3, Visits: 3
I used 2:1 resin/hardener ratio by volumn. 
yudif
yudif
Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)
Group: Awaiting Activation
Posts: 3, Visits: 3
I used 2:1 resin/hardener ratio by volumn. 