Hi, I am new to composite stuff.I am trying to make a small carbon fiber part. But when I lay down my first layer of resin, it doesn't get tacky. I waited for more than 20 mins. I am using
Silmar 249A polyester surfboard resin. Does this resin ever get tacky?Thanks