Hi 

I have made a Carbon arm for a robot in my uni mold form. i have coated the form with GC50 Epoxy Compatible Polyester Gelcoat, bot of some reason i have some holes in the surfase where the cabon epoxy and GC50 Epoxy Compatible Polyester Gelcoat is not glue together . Is it possible to repair it and how
Replies
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Qumec
Qumec
Forum Guru (65 reputation)Forum Guru (65 reputation)Forum Guru (65 reputation)Forum Guru (65 reputation)Forum Guru (65 reputation)Forum Guru (65 reputation)Forum Guru (65 reputation)Forum Guru (65 reputation)Forum Guru (65 reputation)
Group: Forum Members
Posts: 7, Visits: 77
ahh thanks :-)  maby I need a pair of glasses also :-D