Yes you still need to use catalyst with the resin system. All the solution MW does is come to the surface and form a thin layer on the surface of the resin, thus sealing the resin from the air so it can cure hard.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|