Hi 

I have made a Carbon arm for a robot in my uni mold form. i have coated the form with GC50 Epoxy Compatible Polyester Gelcoat, bot of some reason i have some holes in the surfase where the cabon epoxy and GC50 Epoxy Compatible Polyester Gelcoat is not glue together . Is it possible to repair it and how
Reply
Qumec
Qumec
Forum Guru (65 reputation)Forum Guru (65 reputation)Forum Guru (65 reputation)Forum Guru (65 reputation)Forum Guru (65 reputation)Forum Guru (65 reputation)Forum Guru (65 reputation)Forum Guru (65 reputation)Forum Guru (65 reputation)
Group: Forum Members
Posts: 7, Visits: 77
Hi 

Thanks for you help.

Should i use both  Solution MW and the hardner that follows with the GC50 Epoxy Compatible Polyester Gelcoat ?

I am from Denmark, and I Can see that it is not possible to send Solution MW becurse it is dangerous, what can I do? I need it very much, because I need my robot with the exhibition first Febuar in Berlin so I'm a little desperate :-)

Kim 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search