Hi Guys,

I thought I'd pop up and show you what my mate Tim and I are doing with the Easy Composites systems in our garages.

We're what Enzo Ferrari called "Garagistas"  in that we both own AB Performance Sabre race cars, and we build, modify, and prepare them to run  in a race series called  RGB with the 750 motor Club.  In short we're clubman racers and we like building stuff.

Our cars are powered by bike engines, and we aren't allowed wings. so we need to generate aero efficiency from the main body of the car. 

Tim is in mid build of his new Sabre and wanted non standard bodywork to try and improve the aero efficiency, and I wanted different bodywork on my year old Sabre as the car is currently too big to fit in my garage without partially disassembling it, which is a right pain when you arrive home at midnight after a weekends racing.  Also I'm  a big lad and ultra lightweight carbon  bodywork will help me get down to the minimum weight limit for the car and driver.

So we basically decided to build our own bodywork from scratch.   I'd done some small scale fibreglass, buck and mould building in the past on a former car, and we were pretty impressed with the resin infusion process so decided to give the Easy Composites system a try.  We even ran a test infusion process on my glass coffee table top ;-) to make some flat carbon panels.

Although we've never tackled anything of this size, we're doing the full spectrum of build a buck, surface it, then make a mould, them carbon resin infused parts.

So for the last couple of months we've been building a buck around Tim's partially complete chassis.  Well in fact Tim has 90%  of the work and I'm chipping in at weekends.

The buck has been built from timber, 3mm mdf board which is nicely flexible for simple curves, filler and foam. and we're now at the pattern coat primer stage.   We've learned a lot along the way, but basically we've followed the video tutorials and have just scaled up the processes.

Full details are on Tim's website at www.hoverd.org

Details of my racing are at www.rgbracer.com.. and the main AB performance website is www.abperformance.co.uk.

But to whet your appetite here's a picture of the buck in pattern coat.
http://www.hoverd.org/Tim/ttcp/wp-content/uploads/2014/01/Black-again.jpg

Cost to date in materials for the buck, pattern coat, foam etc is about 500 quid, although I've just spent about 600-800 on Unimould materials + CSM  for the mould making stage.

Cheers

Adrian Moore
Edited 11 Years Ago by Ragged99
Replies
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Nice work, is it going on a G1 or a G2 ?

Warren

Carbon Copies Ltd
Teem
Teem
Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)
Group: Forum Members
Posts: 6, Visits: 19
wozza (08/04/2014)
Nice work, is it going on a G1 or a G2 ?

Warren


Both. (He said crossing his fingers...)

T
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Teem (09/04/2014)
wozza (08/04/2014)
Nice work, is it going on a G1 or a G2 ?

Warren


Both. (He said crossing his fingers...)

T


Are you connected to AB or is this totally separate? Had a chance to look over the car whilst exhibiting at Stoneleigh last year, beautifully engineered and some really nice design touches.Smile

Warren

Carbon Copies Ltd
Ragged99
Ragged99
Forum Guru (71 reputation)Forum Guru (71 reputation)Forum Guru (71 reputation)Forum Guru (71 reputation)Forum Guru (71 reputation)Forum Guru (71 reputation)Forum Guru (71 reputation)Forum Guru (71 reputation)Forum Guru (71 reputation)
Group: Forum Members
Posts: 7, Visits: 106
Tim Has a G2 car and mine is a G1.

No we're not linked to AB, except Andy Bates is a mate, and we're both long time happy customers.    The car is indeed beautifully engineered and on a par with much large players in the industry, the quality puts some much better know manufacturers in the shade.

Cheers

Adrian
Ragged99
Ragged99
Forum Guru (71 reputation)Forum Guru (71 reputation)Forum Guru (71 reputation)Forum Guru (71 reputation)Forum Guru (71 reputation)Forum Guru (71 reputation)Forum Guru (71 reputation)Forum Guru (71 reputation)Forum Guru (71 reputation)
Group: Forum Members
Posts: 7, Visits: 106
I should say the complete set of moulds is now complete for the bodywork created so far, including end fences and so on.

So with a first pull of polyester complete we are now ready to rock for the infusion process.

I'm consequently doing  a test of a complex resin infusion shape, in the form of my airbox, for which I'm currently finalising the buck.  Which is incidentally sitting on my G1 bodywork.

Photo: Well I thought I'd finished sanding pattern coat for carbon fibre body parts... But not quite. behold he buck for the new air box constructed from old air box +filler+ elbow grease

This needs to have some returns underneath the shape, and I will clearly need a two part mould for the part because of the recess.

So my plan was to glue the buck on a sheet of melamine board and make a two part mould in the normal way with large flanges sticking out horizontally  from the lower edge as it's shown in the photo.



Then when the mould is made cut another sheet of board  so that it has a hole about 1 inch smaller all around than the footprint of the buck.    This should give me an "internal" return edge.

Cover this second board with release tape.

Then when laying up the mould, tack the carbon down into the top moulds without the base plate in place. and trim back to edge with a couple of inches over lap, and if necessary snip the overhang edges to allow them to fold easily along the return

Before fitting the baseboard , tack some carbon tape in place for the internal flange.  Then fit  the board  and carefully lay the carbon in place from the other half in place.

Then stack and envelope vac bag it in the normal way.

This seems a reasonable plan, but it is a fair bit of a faffing around to get a return edge, .... am I approaching this correctly? 

Will the epoxy infuse up and around the return edges?

If I'm short of time I may go for an external return edge on the normal mould, but this will make fitting it to the parent panel a bit trickier.

Cheers for the help.

Adrian

andygtt
andygtt
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 157, Visits: 1.2K
this is loosely how i do the return edges on my parts... if the areas are hard to get to when the mould is assembled i will often lay it into the mould section carefully and trim it right to the edge, then assemble and overlay the other side around 10mm... then if you do happen to have a void (it happens to me occasionally) then the resin still flows to the carbon edge and often fills the void and you end up with a slightly heavier part but the right shape.... much better than having a bridge that you then have to fill.

great job so far, very impressive

Ragged99 (15/04/2014)



Then when laying up the mould, tack the carbon down into the top moulds without the base plate in place. and trim back to edge with a couple of inches over lap, and if necessary snip the overhang edges to allow them to fold easily along the return
Before fitting the baseboard , tack some carbon tape in place for the internal flange.  Then fit  the board  and carefully lay the carbon in place from the other half in place.

Then stack and envelope vac bag it in the normal way.

This seems a reasonable plan, but it is a fair bit of a faffing around to get a return edge, .... am I approaching this correctly? 

Adrian


y) then the resin still flows to the carbon edge and often fills the void and you end up with a slightly heavier part but the right shape.... much better than having a bridge that you then have to fill.

great job so far, very impressive
Edited 11 Years Ago by andygtt
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Ragged99 - 11 Years Ago
wildcard - 11 Years Ago
Warren (Staff) - 11 Years Ago
Matt (Staff) - 11 Years Ago
Teem - 11 Years Ago
Teem - 11 Years Ago
FLD - 11 Years Ago
Munkee - 11 Years Ago
Warren (Staff) - 11 Years Ago
Teem - 11 Years Ago
Teem - 11 Years Ago
andygtt - 11 Years Ago
Ragged99 - 11 Years Ago
Toffee - 11 Years Ago
Ragged99 - 11 Years Ago
Toffee - 11 Years Ago
Ragged99 - 11 Years Ago
wildcard - 11 Years Ago
Ragged99 - 11 Years Ago
Hanaldo - 11 Years Ago
     Looks great.
wildcard - 11 Years Ago
wozza - 11 Years Ago
Teem - 11 Years Ago
wozza - 11 Years Ago
Ragged99 - 11 Years Ago
Ragged99 - 11 Years Ago
andygtt - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search