I'm using Dremel 3000 along with a diamond wheel which is not cheap either at around 20EUR. It does the trick for about 30-40cm and then goes dull. It only cuts when the dremel is at it's highest setting. Anything less and it barely scratches the surface. It seems as if when the resin is heated while cutting, it sticks on the wheel and dulls it. I don't know if that's whats happening but I can see that the dimond wheel is covered with thick black stuff. I can sand it down with some abrasive paper but that doesn't seem to improve anything. Can anybody help me with that? Any methods for cleaning/sharpening the diamond wheel? 
Reply
macgtech
macgtech
Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)Supreme Being (129 reputation)
Group: Forum Members
Posts: 20, Visits: 102
For long straight cuts, is a bandsaw worthwhile? We will be making some floor sections for one of our cars, and since all the edges will be straight, it seems sensible to get a bandsaw to do the job - does anyone have any experience of this?

MacG Racing Ltd., UK based Motorsport Racing Team - follow us on Twitter and on Facebook
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
StanTheMan - 12 Years Ago
wojtepanik - 12 Years Ago
Brian_s - 12 Years Ago
wojtepanik - 12 Years Ago
Warren (Staff) - 12 Years Ago
baja_patient - 12 Years Ago
dbcrx - 12 Years Ago
StanTheMan - 12 Years Ago
wojtepanik - 12 Years Ago
wojtepanik - 12 Years Ago
dbcrx - 12 Years Ago
macgtech - 11 Years Ago
fgayford - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search