I'm using Dremel 3000 along with a diamond wheel which is not cheap either at around 20EUR. It does the trick for about 30-40cm and then goes dull. It only cuts when the dremel is at it's highest setting. Anything less and it barely scratches the surface. It seems as if when the resin is heated while cutting, it sticks on the wheel and dulls it. I don't know if that's whats happening but I can see that the dimond wheel is covered with thick black stuff. I can sand it down with some abrasive paper but that doesn't seem to improve anything. Can anybody help me with that? Any methods for cleaning/sharpening the diamond wheel? 
Reply
wojtepanik
wojtepanik
Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)
Group: Forum Members
Posts: 102, Visits: 582
StanTheMan (10/12/2013)
Can somebody forward me to a place where they sell those permagrit cutting wheels? I can't seem to find any on eBay...

lol easycomposties.co.uk

~~~Everytime I hear sound of demoulding part I have eargasm~~~
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
StanTheMan - 12 Years Ago
wojtepanik - 12 Years Ago
Brian_s - 12 Years Ago
wojtepanik - 12 Years Ago
Warren (Staff) - 12 Years Ago
baja_patient - 12 Years Ago
dbcrx - 12 Years Ago
StanTheMan - 12 Years Ago
wojtepanik - 12 Years Ago
wojtepanik - 12 Years Ago
dbcrx - 12 Years Ago
macgtech - 11 Years Ago
fgayford - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search